7075 T73 Stress Corrosion Resistant High Strength Aerospace Grade Round Aluminum Bar for Aircraft Structures
Product Details:
| Place of Origin: | China |
| Brand Name: | ECER |
| Certification: | AMS 4124 / ASTM B211 / ISO 9001 |
| Model Number: | 7075-T73-ARB |
Payment & Shipping Terms:
| Minimum Order Quantity: | 500 KG |
|---|---|
| Price: | Negotiation |
| Packaging Details: | Standard Export Seaworthy Packing |
| Delivery Time: | 5~15 DAYS |
| Payment Terms: | T/T,L/C |
| Supply Ability: | 1500 Tons / Month |
|
Detail Information |
|||
| Alloy: | 7075 | Temper: | T73 |
|---|---|---|---|
| Diameter Range: | 10 Mm - 250 Mm | Length: | 1000 Mm - 4000 Mm Or Custom |
| Shape: | Round Bar | Surface Finish: | Mill Finish / Polished |
| Density: | 2.81 G/cm³ | Tensile Strength: | ≥ 470 MPa |
| Yield Strength: | ≥ 390 MPa | Elongation: | ≥ 7% |
| Stress Corrosion Resistance: | Excellent (T73 Overaged) | Application: | Aircraft Structures, Aerospace Fittings, Defense Components |
| Highlight: | 7075 T73 Stress Corrosion Resistant Bar,Aerospace Grade High Strength Aluminum,Aircraft Structural Round Aluminum Bar |
||
Product Description
7075 T73 round aluminum bar combines the exceptional high strength of 7075 alloy with enhanced stress corrosion cracking resistance achieved through the T73 overaging heat treatment. This aerospace-grade material is ideal for aircraft structural components, defense equipment, and high-performance engineering applications where both strength and corrosion reliability are critical.
- Enhanced Stress Corrosion Resistance: T73 overaging treatment significantly improves resistance to stress corrosion cracking compared to T6 temper
- Ultra-High Strength: Tensile strength ≥ 470 MPa, among the highest of all aluminum alloys
- Excellent Fatigue Resistance: Performs reliably under cyclic loading conditions
- Good Machinability: Suitable for precision CNC machining operations
- Aerospace Certified: Meets AMS 4124 specifications
| Item | Specification |
|---|---|
| Alloy | 7075 |
| Temper | T73 |
| Diameter Range | 10 mm - 250 mm |
| Length | 1000 mm - 4000 mm or Custom |
| Standard | AMS 4124 / ASTM B211 |
| Tensile Strength | ≥ 470 MPa |
| Yield Strength | ≥ 390 MPa |
| Elongation | ≥ 7% |
- Aircraft wing spars and fuselage frames
- Aerospace structural fittings and fasteners
- Defense and equipment components
- High-performance racing and motorsport parts
- Precision tooling and mold base plates
The T73 temper involves a two-stage overaging heat treatment that slightly reduces peak strength but dramatically improves resistance to stress corrosion cracking. For aerospace structural applications exposed to corrosive environments or sustained stress, T73 is the recommended temper over T651.