• 7075 T73 Stress Corrosion Resistant High Strength Aerospace Grade Aluminum Round Bar
7075 T73 Stress Corrosion Resistant High Strength Aerospace Grade Aluminum Round Bar

7075 T73 Stress Corrosion Resistant High Strength Aerospace Grade Aluminum Round Bar

Product Details:

Place of Origin: China
Brand Name: ECER
Certification: AMS 4124 / ASTM B211 / ISO 9001
Model Number: 7075-T73-ARB

Payment & Shipping Terms:

Minimum Order Quantity: 500 KG
Price: Negotiation
Packaging Details: Standard Export Seaworthy Packing
Delivery Time: 5~15 DAYS
Payment Terms: T/T,L/C
Supply Ability: 1500 Tons / Month
Get Best Price Contact Now

Detail Information

Alloy: 7075 Temper: T73
Diameter Range: 10 Mm - 250 Mm Length: 1000 Mm - 4000 Mm Or Custom
Shape: Round Bar Surface Finish: Mill Finish / Polished
Density: 2.81 G/cm³ Tensile Strength: ≥ 470 MPa
Yield Strength: ≥ 390 MPa Elongation: ≥ 7%
Stress Corrosion Resistance: Excellent (T73 Overaged) Application: Aircraft Structures, Aerospace Fittings, Defense Components
Highlight:

7075 T73 Stress Corrosion Resistant Bar

,

Aerospace Grade High Strength Aluminum

,

Aircraft Structural Round Aluminum Bar

Product Description

7075 T73 Stress Corrosion Resistant High Strength Aerospace Grade Round Aluminum Bar For Aircraft Structural Components
7075 T73 Stress Corrosion Resistant Round Aluminum Bar
Product Overview

7075 T73 round aluminum bar combines the exceptional high strength of 7075 alloy with enhanced stress corrosion cracking resistance achieved through the T73 overaging heat treatment. This aerospace-grade material is ideal for aircraft structural components, defense equipment, and high-performance engineering applications where both strength and corrosion reliability are critical.

Key Features
  • Enhanced Stress Corrosion Resistance: T73 overaging treatment significantly improves resistance to stress corrosion cracking compared to T6 temper
  • Ultra-High Strength: Tensile strength ≥ 470 MPa, among the highest of all aluminum alloys
  • Excellent Fatigue Resistance: Performs reliably under cyclic loading conditions
  • Good Machinability: Suitable for precision CNC machining operations
  • Aerospace Certified: Meets AMS 4124 specifications
Technical Specifications
Item Specification
Alloy 7075
Temper T73
Diameter Range 10 mm - 250 mm
Length 1000 mm - 4000 mm or Custom
Standard AMS 4124 / ASTM B211
Tensile Strength ≥ 470 MPa
Yield Strength ≥ 390 MPa
Elongation ≥ 7%
Applications
  • Aircraft wing spars and fuselage frames
  • Aerospace structural fittings and fasteners
  • Defense and equipment components
  • High-performance racing and motorsport parts
  • Precision tooling and mold base plates
T73 vs T651: Understanding the Difference

The T73 temper involves a two-stage overaging heat treatment that slightly reduces peak strength but dramatically improves resistance to stress corrosion cracking. For aerospace structural applications exposed to corrosive environments or sustained stress, T73 is the recommended temper over T651.

Frequently Asked Questions
Q: What is the advantage of T73 over T6/T651?
A: T73 provides significantly better resistance to stress corrosion cracking while retaining most of the strength of T6 temper.
Q: Is 7075 T73 suitable for aerospace use?
A: Yes, 7075 T73 is widely specified for aerospace structural components requiring both high strength and corrosion reliability.
Q: Can 7075 T73 be anodized?
A: Yes, anodizing is recommended to further enhance surface protection.
Q: What is the minimum order quantity?
A: MOQ starts at 500 KG. Contact us for bulk pricing.

Want to Know more details about this product
I am interested in 7075 T73 Stress Corrosion Resistant High Strength Aerospace Grade Aluminum Round Bar could you send me more details such as type, size, quantity, material, etc.
Thanks!
Waiting for your reply.